Don't bother sanding 1 coat of high build. Get 3 good coats on it then sand. No need to sand in between. If it's proper UPOL high build stuff out a tin you're using they should be fine after that, although it's hard to say without seeing them up close.
There's no need for more than one coat of etch either, for future reference.